yourstate.us
46 CFR 54.25-25

§ 54.25-25 Welding of quenched and tempered steels (modifies UHT-82).

United States · 46 CFR — Shipping · Status: effective

Get this as JSONEmbed this
Cite this
Citation
46 CFR 54.25-25, § 54.25-25 Welding of quenched and tempered steels (modifies UHT-82), United States, version 1 as recorded 2026-07-09, yourstate.us, https://yourstate.us/provision/225037
Permanent ID
ys:prov:225037@1
SHA-256
8e111e512c48814f0619d25cda6689c545a5b0d166268ac400e8c295cb4fa508

The hash is SHA-256 of this version's text, with every run of whitespace collapsed to a single space and the ends trimmed. The ID always leads back here, and checking it says whether the text you cited is still the current version.

Full text

(a) The qualification of welding procedures, welders, and weld-production testing must conform to the requirements of part 57 of this subchapter. The requirements of § 57.03-1(d) of this subchapter apply to welded pressure vessels and non-pressure vessel type tanks of quenched and tempered steels other than 9-percent nickel. (b) [Reserved]

Legislative history