46 CFR 154.450
§ 154.450 General.
United States · 46 CFR — Shipping · Status: effective
Cite this
- Citation
- 46 CFR 154.450, § 154.450 General, United States, version 1 as recorded 2026-07-09, yourstate.us, https://yourstate.us/provision/228901
- Permanent ID
ys:prov:228901@1- SHA-256
fb7cc20bd539ba375ff2b1248c3bba4bcadf4f4b49ff8cbbd318e640859725ae
The hash is SHA-256 of this version's text, with every run of whitespace collapsed to a single space and the ends trimmed. The ID always leads back here, and checking it says whether the text you cited is still the current version.
Full text
Independent tanks type C and process pressure vessels must be designed to meet the requirements under Part 54 of this chapter, except § 54.01-40(b), and:
(a) The calculation under § 54.01-18 (b)(1) must also include the design loads determined under § 154.406;
(b) The calculated tank plating thickness, including any corrosion allowance, must be the minimum thickness without a negative plate tolerance; and
(c) The minimum tank plating thickness must not be less than:
(1) 5mm ( 3/16 in.) for carbon-manganese steel and nickel steel;
(2) 3mm ( 1/8 in.) for austenitic steels; or
(3) 7mm ( 9/32 in.) for aluminum alloys.