yourstate.us
46 CFR 164.003-4

§ 164.003-4 Inspections and tests.

United States · 46 CFR — Shipping · Status: effective

Get this as JSONEmbed this
Cite this
Citation
46 CFR 164.003-4, § 164.003-4 Inspections and tests, United States, version 1 as recorded 2026-07-09, yourstate.us, https://yourstate.us/provision/229781
Permanent ID
ys:prov:229781@1
SHA-256
d0a1e606c6865a2b2f20da41ba93a0f8d7732e4c6a9a17d7de50a0167e5b56d8

The hash is SHA-256 of this version's text, with every run of whitespace collapsed to a single space and the ends trimmed. The ID always leads back here, and checking it says whether the text you cited is still the current version.

Full text

(a) Kapok fibers to be used in a finished product subject to inspection by the Coast Guard shall be subject to inspection and tests at the plant of the manufacturer of such product, who shall furnish the necessary testing tank, test cages, and scales. (b) Acceptance of kapok prior to being incorporated into finished products, or during the course of manufacture, shall in no case be construed as a guarantee of the acceptance of the finished product. (c) Not less than a one-pound sample from each 1,000 pounds of kapok shall be tested for buoyancy by the inspector. At his discretion, the inspector may select additional samples for tests if deemed advisable. (d) The buoyancy test shall be made with 16 ounces of processed kapok uniformly packed in a rigid wire box or cage with metal reinforced edges, and submerged by weights in a tank of fresh water to a depth of 12 inches below the surface of the water, measurement made to the top of box, for 48 hours. The test box shall be cylindrical in shape, and as nearly as practicable 1/3 cubic foot in volume, 4 inches deep, 13.54 inches diameter, all inside measurements; constructed of about 0.065 inch galvanized iron wire with about 1/4 inch mesh, and lined with about 0.007 inch copper wire screen about 18 meshes to the inch, to prevent the kapok from pushing out through the larger wire meshes. At the end of forty-eight hours submergence, the buoyancy shall be determined by subtracting the submerged weight of the box, accessory weights and kapok from the submerged weight of the box and weights without the kapok, and dividing the remainder by the volume of the kapok expressed in cubic feet. (e) Kapok fiber shall, at the option of the inspector, be subjected to a microscopic examination to detect adulteration with other fiber. (f) Processed kapok shall, at the option of the inspector, be subjected to separation of kapok fibers from foreign matter by hand, the portions of each weighed, and percentage of foreign matter computed for compliance with § 164.003-3(d).