49 CFR 179.100-10
§ 179.100-10 Postweld heat treatment.
United States · 49 CFR — Transportation · Status: effective
Cite this
- Citation
- 49 CFR 179.100-10, § 179.100-10 Postweld heat treatment, United States, version 1 as recorded 2026-07-09, yourstate.us, https://yourstate.us/provision/256708
- Permanent ID
ys:prov:256708@1- SHA-256
9c82e7ff897b9246503627da3b4602a0501375281a098e72dbd4f8d1805c3d52
The hash is SHA-256 of this version's text, with every run of whitespace collapsed to a single space and the ends trimmed. The ID always leads back here, and checking it says whether the text you cited is still the current version.
Full text
(a) After welding is complete, steel tanks and all attachments welded thereto must be postweld heat treated as a unit in compliance with the requirements of AAR Specifications for Tank Cars, appendix W (IBR, see § 171.7 of this subchapter).
(b) For aluminum tanks, postweld heat treatment is prohibited.
(c) Tank and welded attachments, fabricated from ASTM A 240/A 240M (IBR, see § 171.7 of this subchapter), Type 304L or Type 316L materials do not require postweld heat treatment, but these materials do require a corrosion resistance test as specified in § 179.100-7(c)(2).