§ 192.489 Remedial measures: Cast iron and ductile iron pipelines.

United States · 49 CFR — Transportation · Status: effective

Get this as JSONEmbed this
Cite this
Citation
49 CFR 192.489, § 192.489 Remedial measures: Cast iron and ductile iron pipelines, United States, version 1 as recorded 2026-07-09, yourstate.us, https://yourstate.us/provision/257170
Permanent ID
ys:prov:257170@1
SHA-256
638a582a317ecb1aa3e88eea165c7853c9f6338738d0f40151d669ce60b0192a

The hash is SHA-256 of this version's text, with every run of whitespace collapsed to a single space and the ends trimmed. The ID always leads back here, and checking it says whether the text you cited is still the current version.

Full text

(a) General graphitization. Each segment of cast iron or ductile iron pipe on which general graphitization is found to a degree where a fracture or any leakage might result, must be replaced. (b) Localized graphitization. Each segment of cast iron or ductile iron pipe on which localized graphitization is found to a degree where any leakage might result, must be replaced or repaired, or sealed by internal sealing methods adequate to prevent or arrest any leakage.