§ 195.226 Welding: Arc burns.

United States · 49 CFR — Transportation · Status: effective

Get this as JSONEmbed this
Cite this
Citation
49 CFR 195.226, § 195.226 Welding: Arc burns, United States, version 1 as recorded 2026-07-09, yourstate.us, https://yourstate.us/provision/257495
Permanent ID
ys:prov:257495@1
SHA-256
296a7f426668572f01a50267ea1f97f49f23c4c35007e511e9f48acf017f23e9

The hash is SHA-256 of this version's text, with every run of whitespace collapsed to a single space and the ends trimmed. The ID always leads back here, and checking it says whether the text you cited is still the current version.

Full text

(a) Each arc burn must be repaired. (b) An arc burn may be repaired by completely removing the notch by grinding, if the grinding does not reduce the remaining wall thickness to less than the minimum thickness required by the tolerances in the specification to which the pipe is manufactured. If a notch is not repairable by grinding, a cylinder of the pipe containing the entire notch must be removed. (c) A ground may not be welded to the pipe or fitting that is being welded.